Differential Scanning Calorimeters : Differential Scanning Calorimeter LDSC-A11


Share :



Differential Scanning Calorimeter LDSC-A11 is an analyzer which allows the measurement of different characteristic properties of various samples from RT to 600°C. It meets ASTM, ISO standards. High resolution, stable base line, air flow meter, bilateral control etc. are some of the features which ensures accurate and reliable results. It finds applications in fields like polymer development, quality control of different materials, performance testing and many other industries.



Available Range :

Temperature range : RT to 800°C (Air cooled) Temperature range : RT to 600°C (Air cooled) Temperature range : -150°C to 550°C
Temperature rangeRT to 600°C (Air cooled)
Temperature resolution0.1°C
Temperature fluctuations± 0.1°C
Temperature repeatability± 0.1°C
Dynamic heat flow range (DSC range)0 to ± 500 mW
Heating rate1 to 80°C / min
Cooling rate1 to 20°C / min
DSC noise0.01 μW
DSC resolution0.01 µW
DSC accuracy0.1 µW
DSC sensitivity0.1 µW
Control ModeRising temperature, constant temperature (full automatic)
Curve scanningRising scan, cooling scan
Gas flow controlEmbedded digital flow meter & Software control, automatic changing
Parameter standardWith standard material, with calibration function, the user may correct temperature and heat enthalpy
Display24 bit 7 inches LCD touch screen display
Data interfaceStandard USB connector
Power ConsumptionLess than 2000 W
Packaging Dimension and Gross weight (2 case)580×490×520 mm / 29 kg
530×270×280 mm / 15 kg
  • Renewed design of oven structure
  • High stability and resolution of base line
  • Accurate control of air flow rate
  • Test data storage function
  • Both main frame and software control option
  • LCD touch screen display
  • Meets ISO and ASTM standards
It is used to study thermal transitions, heat capacity, glass transition temperature, crystallinity, melting temperature etc. of various materials like polymers, plastics, elastomer, food stuffs, biomolecules, non-corrosive samples, electronic components etc.
Name of Accessories Quantity
Host instrument 1
CD 1
Data Line 1
Power Line 1
Aluminium crucibles 100
Ceramic crucibles 100
pure tin grains 1bag
Fuse 4A 5

Differential Scanning Calorimeters

Differential Scanning Calorimeters : Differential Scanning Calorimeter LDSC-A10

Differential Scanning Calorimeter LDSC-A10

  • Temperature range
  • RT to 800°C (Air cooled)
  • Temperature resolution
  • 0.1°C
  • Temperature fluctuations
  • ± 0.1°C
Differential Scanning Calorimeters : Differential Scanning Calorimeter LDSC-A12

Differential Scanning Calorimeter LDSC-A12

  • Temperature range
  • -150°C to 550°C
  • Temperature resolution
  • 0.001°C
  • Temperature fluctuations
  • ± 0.001°C