Differential Scanning Calorimeter LDSC-A10
| Differential Scanning Calorimeter LDSC-A10 is an analyzer which allows the measurement of different characteristic properties of various samples from RT to 800°C. It meets ASTM, ISO standards. High resolution, stable base line, air flow meter, bilateral control etc. are some of the features which ensures accurate and reliable results. It finds applications in fields like polymer development, quality control of different materials, performance testing and many other industries. |
| Temperature range | RT to 800°C (Air cooled) |
| Temperature resolution | 0.1°C |
| Temperature fluctuations | ± 0.1°C |
| Temperature repeatability | ± 0.1°C |
| Dynamic heat flow range (DSC range) | 0 to ± 500 mW |
| Heating rate | 1 to 80°C / min |
| Cooling rate | 1 to 20°C / min (OPTIONAL) |
| DSC noise | 0.01 μW |
| DSC resolution | 0.01 µW |
| DSC accuracy | 0.1 µW |
| DSC sensitivity | 0.1 µW |
| Control Mode | Rising temperature, constant temperature (full automatic) |
| Curve scanning | Rising scan, cooling scan(OPTIONAL) |
| Gas flow control | Embedded digital flow meter & Software control, automatic changing |
| Parameter standard | With standard material, with calibration function, the user may correct temperature and heat enthalpy |
| Display | 24 bit 7 inches LCD touch screen display |
| Data interface | Standard USB connector |
| Power Consumption | Less than 2000 W |
| Packaging Dimension and Gross weight (2 case) |
580×490×520 mm / 29 kg 530×270×280 mm / 15 kg |
Features :
|
Applications :It is used to study thermal transitions, heat capacity, glass transition temperature, crystallinity, melting temperature etc. of various materials like polymers, plastics, elastomer, food stuffs, biomolecules, non-corrosive samples, electronic components etc. |